Disperse Rubine WECT 200%Product advantages of disperse Rubine WECT 200%Good leveling property, bright color, and darker color can be dyed;The dyed yarn has a soft feel and smooth fabric.Product application of disperse Rubine WECT 200%Mainly used for printing and dyeing polyester and its blended fab......
Good leveling property, bright color, and darker color can be dyed;The dyed yarn has a soft feel and smooth fabric.
Mainly used for printing and dyeing polyester and its blended fabrics. It can also be used for the printing and dyeing of synthetic fibers such as acetate, nylon, polypropylene, chlorinated fiber, and acrylic fiber.
0.30.60.91.21.51.82.12.42.73.0
Heating rate 1.0℃/min 2.0%(o.w.f)
Temperature70℃80℃90℃100℃110℃120℃130℃130℃*20min130℃*40min80℃
Heating
Raffinate
Dye bath PH value34567891011
Disperse Rubine WECT
Rubine Raffinate
PH value after dyeing3.164.165.246.296.747.207.337.417.61
4.1 Washing Fastness:AATCC-61-2A(Six fiber cloth 49℃×45min)
Formula (o.w.f)Rubine WECTCategoryBeforetestAftertestWOPACPESPACOCAFormula (o.w.f)Rubine WECTCategoryBeforetestAftertestWOPACPESPACOCA
0.3%UnreducedWashing2.1%UnreducedWashing
LevelLevel
0.3%ReductionWashing2.1%ReductionWashing
LevelLevel
0.9%UnreducedWashing2.7%UnreducedWashing
LevelLevel
0.9%ReductionWashing2.7%ReductionWashing
LevelLevel
1.5%UnreducedWashing3.0%UnreducedWashing
LevelLevel
1.5%ReductionWashing3.0%ReductionWashing
LevelLevel
4.2 Washing Fastness:GB/T3921-C 60℃×30min
Unreduced washReduction wash
Formula (o.w.f)Rubine WECTCategoryBeforetestAftertestWOPACPESPACOCAFormula (o.w.f)Rubine WECTCategoryBeforetestAftertestWOPACPESPACOCA
0.3%UnreducedWashing0.3%UnreducedWashing
LevelLevel
0.6%ReductionWashing0.6%ReductionWashing
LevelLevel
1.5%UnreducedWashing1.5%UnreducedWashing
LevelLevel
2.1%ReductionWashing2.1%ReductionWashing
LevelLevel
2.7%UnreducedWashing2.7%UnreducedWashing
LevelLevel
3.0%ReductionWashing3.0%ReductionWashing
LevelLevel
4.3 Spell white fastness:60℃×30min (Unreduced wash)
Formula(o.w.f)BeforetestAftertestStainingFormula(o.w.f)BeforetestAftertestStaining
Rubine WECT0.3%Rubine WECT2.1%
LevelLevel
Rubine WECT0.9%Rubine WECT2.7%
LevelLevel
Rubine WECT1.5%Rubine WECT3.0%
LevelLevel
Spell white fastness: 60℃×30min (Reduction wash)
Formula(o.w.f)BeforetestAftertestStainingFormula(o.w.f)BeforetestAftertestStaining
Rubine WECT0.3%Rubine WECT2.1%
levellevel
Rubine WECT0.9%Rubine WECT2.7%
levellevel
Rubine WECT1.5%Rubine WECT3.0%
levellevel
4.4 Sublimation Fastness:ISO-105-P01(Pure polyester/cotton standard interlining,180℃×30s)
formula (o.w.f)Rubine WECTBeforetestAftertestPESCOformula (o.w.f)Rubine WECTBeforetestAftertestPESCO
0.3%(Unreduced wash)2.1%(Unreduced wash)
levellevel
0.3%(Reduction wash)2.1%(Reduction wash)
levellevel
0.9%(Unreduced wash)2.7%(Unreduced wash)
levellevel
0.9%(Reduction wash)2.7%(Reduction wash)
levellevel
1.5%(Unreduced wash)3.0%(Unreduced wash)
levellevel
1.5%(Reduction wash)3.0%(Reduction wash)
levellevel
4.5 Bubble Water Fastness:(3g/L washing powder 70℃×1min)
formulao.w.f)BlankRubine WECT0.3%Rubine WECT0.9%Rubine WECT1.5%Rubine WECT2.1%Rubine WECT2.7%Rubine WECT3.0%
(Unrestored)Fade
LevelBlank43-43-432-32-3
(Restored)Fade
LevelBlank4-54-5443-43-4
Dyeing condition
dyeing processHPHT
fabricsKnitted polyester cloth
acetic acid0.5g/L
levelling agent0.5g/L
liquor ratio1:20
dye bath PH valuePH=4
temperature130℃×40min
Reduction washing Conditions
sodium hydrosulflte4g/L
caustic soda fiake3g/L
temperature80℃×20min
1 We have our own factory, R&D center and laboratory.
2 We can provide product customization services and technical support according to customer needs.
6mm thick five-layer 25KG corrugated box.